{"id":18813,"date":"2026-08-04T09:57:17","date_gmt":"2026-08-04T01:57:17","guid":{"rendered":"https:\/\/rysilicone.com\/?p=18813"},"modified":"2026-08-05T17:12:44","modified_gmt":"2026-08-05T09:12:44","slug":"silicone-density-hydrophobicity","status":"publish","type":"post","link":"https:\/\/rysilicone.com\/it\/silicone-density-hydrophobicity\/","title":{"rendered":"Densit\u00e0 del silicone: il silicone galleggia ed \u00e8 resistente all&#039;acqua?"},"content":{"rendered":"<p class=\"wp-block-paragraph\">Il silicone viene spesso descritto come leggero, impermeabile e idrofobico. \u00c8 facile confondere questi termini. <strong>La densit\u00e0 tipica del silicone solido \u00e8 di circa 1,05\u20131,60 g\/cm\u00b3, quindi la maggior parte dei componenti in silicone non espanso affonda in acqua. L&#039;idrofobicit\u00e0 fa s\u00ec che l&#039;acqua formi gocce sulla superficie, ma non rende ogni oggetto in silicone a tenuta stagna o impermeabile.<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Nella progettazione del prodotto, sono fondamentali tre aspetti distinti: la densit\u00e0 del composto, la densit\u00e0 media dell&#039;intero componente e il modo in cui l&#039;acqua interagisce con la superficie e la geometria della guarnizione.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Qual \u00e8 la densit\u00e0 tipica del silicone?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">La densit\u00e0 di una mescola di gomma siliconica vulcanizzata \u00e8 data dalla sua massa divisa per il suo volume. Viene solitamente espressa in g\/cm\u00b3, kg\/m\u00b3 o come peso specifico.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Per molti solidi <a href=\"https:\/\/rysilicone.com\/it\/high-temperature-vulcanizing-silicone-rubber\/\">composti HCR<\/a> E <a href=\"https:\/\/rysilicone.com\/it\/liquid-silicone-rubber\/\">Composti LSR<\/a>, un intervallo di partenza pratico \u00e8 <strong>1,05\u20131,60 g\/cm\u00b3<\/strong>. WACKER riporta questo intervallo per la gomma siliconica e osserva che ulteriori riempitivi inattivi come il quarzo possono aumentare la densit\u00e0 a circa <strong>1,75 g\/cm\u00b3<\/strong>. I singoli composti speciali possono rientrare al di fuori di questo intervallo, pertanto il valore di riferimento rimane quello riportato nella scheda tecnica del materiale approvato.<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Materiale o costruzione in silicone<\/th><th>Intervallo di densit\u00e0 pratico<\/th><th>Tendenza alla galleggiabilit\u00e0 in acqua dolce<\/th><th>Motivo principale della variazione<\/th><\/tr><\/thead><tbody><tr><td>Gomma siliconica solida per uso generale<\/td><td>1,05\u20131,30 g\/cm\u00b3<\/td><td>Di solito i lavandini<\/td><td>Polimero, silice di rinforzo, pigmento e additivi<\/td><\/tr><tr><td>mescola siliconica ad alto contenuto di riempitivo<\/td><td>1,30\u20131,75+ g\/cm\u00b3<\/td><td>Lavandini<\/td><td>Quarzo, ossido metallico o altro riempitivo ad alta densit\u00e0<\/td><\/tr><tr><td>Fluorosilicone o composto speciale<\/td><td>Specifico per grado scolastico<\/td><td>Di solito i lavandini<\/td><td>Diverse confezioni di polimeri e riempitivi<\/td><\/tr><tr><td>Gommapiuma o spugna di silicone<\/td><td>Spesso inferiore a 1,0 g\/cm\u00b3<\/td><td>Potrebbe galleggiare<\/td><td>Struttura cellulare chiusa o aperta<\/td><\/tr><tr><td>Parte cava in silicone stampato<\/td><td>Dipende dalla massa totale e dal volume spostato.<\/td><td>Potrebbe galleggiare<\/td><td>L&#039;aria intrappolata riduce la densit\u00e0 media del componente.<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Questi sono intervalli di progetto, non limiti di controllo in entrata. Per gli acquisti e il controllo qualit\u00e0, specificare la densit\u00e0 indicata nella scheda tecnica approvata e definire il metodo di prova.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Densit\u00e0 e peso specifico sono la stessa cosa?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Sono strettamente imparentati, ma non identici.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Densit\u00e0<\/strong> \u00e8 la massa per unit\u00e0 di volume. <strong>Peso specifico<\/strong> \u00c8 il rapporto tra la densit\u00e0 di un materiale e la densit\u00e0 dell&#039;acqua a una determinata temperatura. Poich\u00e9 la densit\u00e0 dell&#039;acqua \u00e8 vicina a 1,00 g\/cm\u00b3, i valori numerici sono spesso simili quando la densit\u00e0 viene espressa in g\/cm\u00b3.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Un composto siliconico con una densit\u00e0 di 1,20 g\/cm\u00b3 ha quindi un peso specifico prossimo a 1,20 in condizioni di prova ordinarie.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Per i componenti in silicone solido, i metodi di misurazione pi\u00f9 comuni includono:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>ASTM D792<\/strong> per densit\u00e0 e peso specifico mediante spostamento<\/li>\n\n\n\n<li><strong>Metodo A della norma ISO 1183-1<\/strong> per la misurazione dell&#039;immersione<\/li>\n\n\n\n<li><strong>ASTM D297<\/strong> metodi utilizzati per prodotti e mescole di gomma<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">Il metodo, le condizioni del campione, la temperatura e la presenza di bolle intrappolate influenzano il risultato. Confrontare i dati dei fornitori senza verificare il metodo pu\u00f2 generare una differenza falsata.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Il silicone galleggia in acqua?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">La maggior parte della gomma siliconica solida non espansa affonda perch\u00e9 la sua densit\u00e0 \u00e8 superiore a quella dell&#039;acqua dolce.<\/p>\n\n\n\n<figure class=\"wp-block-image size-large\"><img fetchpriority=\"high\" decoding=\"async\" width=\"1024\" height=\"572\" src=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats-1024x572.jpg\" alt=\"\" class=\"wp-image-18818\" srcset=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats-1024x572.jpg 1024w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats-300x167.jpg 300w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats-768x429.jpg 768w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats-18x10.jpg 18w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats-600x335.jpg 600w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Solid-silicone-sinks-while-hollow-silicone-part-floats.jpg 1376w\" sizes=\"(max-width: 1024px) 100vw, 1024px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">La condizione fondamentale \u00e8:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>Se la densit\u00e0 media delle parti \u00e8 <strong>inferiore a 1,00 g\/cm\u00b3<\/strong>, la parte pu\u00f2 galleggiare in acqua dolce.<\/li>\n\n\n\n<li>Se la densit\u00e0 media delle parti \u00e8 <strong>superiore a 1,00 g\/cm\u00b3<\/strong>, il pezzo affonda a meno che la sua geometria non intrappoli abbastanza aria.<\/li>\n\n\n\n<li>Nell&#039;acqua salata, la densit\u00e0 del liquido \u00e8 maggiore, quindi la stessa parte riceve una forza di galleggiamento leggermente superiore.<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">SIMTEC riporta una densit\u00e0 LSR tipica di <strong>1,10\u20131,50 g\/cm\u00b3<\/strong> e nota che l&#039;LSR solido affonda quindi. La parola importante \u00e8 <em>solido<\/em>. Un giocattolo da bagno cavo, un galleggiante sigillato o un assemblaggio sovrastampato possono galleggiare anche se il loro rivestimento in silicone \u00e8 pi\u00f9 denso dell&#039;acqua.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">Esempio di silicone solido<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Un componente in silicone solido ha:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>Volume: 100 cm\u00b3<\/li>\n\n\n\n<li>Densit\u00e0 del composto: 1,20 g\/cm\u00b3<\/li>\n\n\n\n<li>Massa: 100 \u00d7 1,20 = 120 g<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">Quando \u00e8 completamente immerso, sposta circa 100 g di acqua dolce. Il pezzo pesa pi\u00f9 dell&#039;acqua spostata, quindi affonda.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">esempio di silicone cavo<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Si supponga che una parte sigillata pesi 70 g e sposti 150 cm\u00b3 di acqua in base al suo volume esterno.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Densit\u00e0 media dei pezzi = 70 \u00f7 150 = <strong>0,47 g\/cm\u00b3<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">La cavit\u00e0 d&#039;aria sigillata riduce la densit\u00e0 dell&#039;intero assemblaggio al di sotto di quella dell&#039;acqua, consentendo al componente di galleggiare. Se la cavit\u00e0 perde e si riempie d&#039;acqua, questo vantaggio scompare.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Quanto pesa un componente in silicone?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Utilizzare la densit\u00e0 del composto finito, non un valore generico del silicone.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Massa = volume \u00d7 densit\u00e0<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Per le dimensioni in millimetri:<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Massa (g) = volume (mm\u00b3) \u00f7 1.000 \u00d7 densit\u00e0 (g\/cm\u00b3)<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Un cuscinetto rettangolare in silicone di dimensioni 100 \u00d7 50 \u00d7 5 mm ha un volume di 25.000 mm\u00b3, ovvero 25 cm\u00b3. Con una densit\u00e0 di 1,20 g\/cm\u00b3, la massa stimata \u00e8:<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">25 \u00d7 1,20 = <strong>30 g<\/strong><\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Ingresso<\/th><th>Esempio di valore<\/th><th>Rischio di approvvigionamento se assunto<\/th><\/tr><\/thead><tbody><tr><td>Volume netto stampato<\/td><td>25 cm\u00b3<\/td><td>Il volume CAD potrebbe escludere nervature, canali di accesso o inserti.<\/td><\/tr><tr><td>Densit\u00e0 del composto<\/td><td>1,20 g\/cm\u00b3<\/td><td>Una formulazione sostitutiva modifica il peso del pezzo<\/td><\/tr><tr><td>Massa stimata della parte<\/td><td>30 g<\/td><td>Le stime relative all&#039;imballaggio e al trasporto possono variare per ordini di grandi dimensioni.<\/td><\/tr><tr><td>Quantit\u00e0 dell&#039;ordine<\/td><td>100.000 pezzi<\/td><td>Un errore di 2 g diventa 200 kg sull&#039;intera spedizione<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Questo calcolo \u00e8 utile per la formulazione di preventivi e stime di imballaggio. I limiti di peso finali per singolo pezzo dovrebbero essere ricavati da campioni validati, poich\u00e9 le sbavature, il peso dell&#039;inserto, il pigmento, il contenuto di riempitivo e le variazioni di stampaggio rimangono nel pezzo finito.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Quali fattori influenzano la densit\u00e0 del silicone?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">La densit\u00e0 del silicone dipende dalla formulazione. Non \u00e8 determinata unicamente dal nome del polimero.<\/p>\n\n\n\n<figure class=\"wp-block-image size-large\"><img decoding=\"async\" width=\"1024\" height=\"572\" src=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors-1024x572.jpg\" alt=\"\" class=\"wp-image-18814\" srcset=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors-1024x572.jpg 1024w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors-300x167.jpg 300w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors-768x429.jpg 768w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors-18x10.jpg 18w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors-600x335.jpg 600w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Silicone-fillers-pigments-and-foam-density-factors.jpg 1376w\" sizes=\"(max-width: 1024px) 100vw, 1024px\" \/><\/figure>\n\n\n\n<h3 class=\"wp-block-heading\">Cariche di rinforzo e inattive<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">La silice pirogenica o precipitata rinforza il polimero. Il quarzo e altri riempitivi minerali possono aumentarne ulteriormente la densit\u00e0. Un compounder pu\u00f2 utilizzare riempitivi per regolare la durezza, la resistenza allo strappo, la reologia, il comportamento elettrico, la resistenza al rigonfiamento o il costo. <a href=\"https:\/\/rysilicone.com\/it\/silicone-shore-hardness\/\">Durezza Shore A<\/a> Pertanto, \u00e8 possibile ottenerli con diverse formulazioni e diverse densit\u00e0.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">Pigmenti e additivi funzionali<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Il masterbatch di colore solitamente provoca una variazione minore rispetto a un elevato carico di riempitivo, ma l&#039;effetto \u00e8 misurabile quando le tolleranze di peso del pezzo sono ristrette. Gli additivi ignifughi, termoconduttivi, elettricamente conduttivi o radiopachi possono modificare sostanzialmente la densit\u00e0.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">Aria, vuoti e struttura cellulare<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Il silicone espanso contiene celle di gas e pu\u00f2 avere una densit\u00e0 apparente inferiore a 1,00 g\/cm\u00b3. Anche i vuoti indesiderati possono ridurre la densit\u00e0 misurata di un campione, ma questo \u00e8 un segnale di difetto piuttosto che una valida via per la riduzione del peso.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">Controllo della cura e del processo<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Le condizioni di polimerizzazione hanno normalmente un&#039;influenza minore sulla densit\u00e0 rispetto alla formulazione, ma errori di miscelazione, un rapporto A:B errato per LSR, contaminazione o aria intrappolata possono alterare i valori misurati. La densit\u00e0 \u00e8 quindi utile come rapido controllo preliminare, non come prova che ogni propriet\u00e0 meccanica o di conformit\u00e0 sia corretta.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Il silicone \u00e8 idrofobico?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Il silicone a base di PDMS non trattato \u00e8 intrinsecamente idrofobico perch\u00e9 i gruppi metilici si orientano sulla sua superficie a bassa energia. L&#039;acqua tende a formare gocce invece di diffondersi su una superficie <a href=\"https:\/\/rysilicone.com\/it\/silicone-sheet\/\">foglio di silicone<\/a>.<\/p>\n\n\n\n<figure class=\"wp-block-image size-large\"><img decoding=\"async\" width=\"1024\" height=\"572\" src=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface-1024x572.jpg\" alt=\"\" class=\"wp-image-18819\" srcset=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface-1024x572.jpg 1024w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface-300x167.jpg 300w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface-768x429.jpg 768w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface-18x10.jpg 18w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface-600x335.jpg 600w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Water-droplet-showing-a-hydrophobic-silicone-surface.jpg 1376w\" sizes=\"(max-width: 1024px) 100vw, 1024px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Un angolo di contatto con l&#039;acqua comunemente riportato per il PDMS non trattato \u00e8 di circa <strong>100\u2013120\u00b0<\/strong>. Le misurazioni pubblicate variano in base alla formulazione, alla rugosit\u00e0 della superficie, alla pulizia, al metodo di deposizione delle gocce e al condizionamento. Un angolo di contatto superiore a 90\u00b0 indica generalmente un comportamento di bagnatura idrofobica.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">L&#039;idrofobicit\u00e0 descrive l&#039;interazione della superficie con una goccia d&#039;acqua. Non descrive il comportamento completo di un prodotto stampato.<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Propriet\u00e0<\/th><th>Cosa misura<\/th><th>Ci\u00f2 che non dimostra<\/th><\/tr><\/thead><tbody><tr><td>angolo di contatto dell&#039;acqua<\/td><td>Bagnabilit\u00e0 della superficie<\/td><td>Resistenza alle perdite di un assemblaggio<\/td><\/tr><tr><td>Assorbimento dell&#039;acqua<\/td><td>Aumento di massa dopo un periodo di esposizione definito<\/td><td>comportamento di formazione di gocce sulla superficie<\/td><\/tr><tr><td>permeabilit\u00e0 al vapore acqueo<\/td><td>Trasporto di umidit\u00e0 attraverso il materiale<\/td><td>Resistenza alla perdita di acqua liquida in una giunzione<\/td><\/tr><tr><td>Grado di protezione IP<\/td><td>Protezione dell&#039;involucro secondo un test definito<\/td><td>Prestazioni universali a qualsiasi pressione e durata<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Anche il trattamento superficiale influisce sul risultato. Il trattamento al plasma di ossigeno o a corona pu\u00f2 rendere temporaneamente il PDMS pi\u00f9 idrofilo, migliorando l&#039;adesione, il rivestimento o la bagnabilit\u00e0 microfluidica. Le superfici in silicone possono quindi recuperare la loro idrofobia nel tempo. Pertanto, le prove di adesione dovrebbero definire il tempo consentito tra il trattamento e l&#039;applicazione dell&#039;adesivo.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Il silicone \u00e8 impermeabile?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Un componente continuo in silicone \u00e8 generalmente resistente all&#039;acqua liquida, ma la dicitura &quot;impermeabile&quot; si riferisce al sistema piuttosto che alla propriet\u00e0 del materiale di base.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Una guarnizione stampata pu\u00f2 comunque perdere quando:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>La compressione \u00e8 troppo bassa o irregolare;<\/li>\n\n\n\n<li>la linea di separazione attraversa la superficie di tenuta;<\/li>\n\n\n\n<li>bagliori, linee di lavorazione, polvere o danni superficiali creano un percorso di infiltrazione;<\/li>\n\n\n\n<li>La deformazione permanente da compressione riduce la forza di tenuta nel corso di ripetuti cicli termici;<\/li>\n\n\n\n<li>l&#039;alloggiamento si flette sotto pressione;<\/li>\n\n\n\n<li>Il design del giunto si basa su un adesivo che non bagna il silicone non trattato;<\/li>\n\n\n\n<li>L&#039;involucro viene testato a una pressione o per una durata al di fuori dei suoi limiti di progetto.<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">Spesso i team sovrastimano l&#039;idrofobicit\u00e0 perch\u00e9 la presenza di gocce d&#039;acqua visibili sembra una prova di tenuta. In fase di produzione, il percorso della perdita si trova solitamente all&#039;interfaccia, non al centro di una sezione di silicone integra.<\/p>\n\n\n\n<figure class=\"wp-block-image size-large\"><img loading=\"lazy\" decoding=\"async\" width=\"1024\" height=\"572\" src=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure-1024x572.jpg\" alt=\"\" class=\"wp-image-18820\" srcset=\"https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure-1024x572.jpg 1024w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure-300x167.jpg 300w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure-768x429.jpg 768w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure-18x10.jpg 18w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure-600x335.jpg 600w, https:\/\/rysilicone.com\/wp-content\/uploads\/2026\/08\/Compressed-silicone-gasket-blocking-water-under-pressure.jpg 1376w\" sizes=\"(max-width: 1024px) 100vw, 1024px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Per un involucro, definire il requisito effettivo: esposizione a spruzzi, immersione continua, pressione idrostatica, vapore, acqua salata, prodotti chimici per la pulizia o test IP. Queste condizioni non sono intercambiabili.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Quanta acqua assorbe il silicone?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">La gomma siliconica in genere ha un basso assorbimento d&#039;acqua, ma un valore universale come &quot;inferiore a 0,5%&quot; non dovrebbe essere applicato a ogni mescola.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">I database pubblicati contengono un&#039;ampia gamma perch\u00e9 combinano gomma densa, schiuma, formulazioni speciali, diversi spessori dei campioni e diverse condizioni di esposizione. L&#039;assorbimento d&#039;acqua deve quindi essere legato a un grado e a un metodo come <strong>ASTM D570<\/strong> O <strong>ISO 62<\/strong>, con la durata e la temperatura indicate.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Per una specifica completa, si prega di richiedere:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>il grado testato e le condizioni di polimerizzazione;<\/li>\n\n\n\n<li>spessore del campione;<\/li>\n\n\n\n<li>tempo di immersione e temperatura dell&#039;acqua;<\/li>\n\n\n\n<li>variazione percentuale di massa;<\/li>\n\n\n\n<li>variazione dimensionale, se le tolleranze ristrette sono importanti;<\/li>\n\n\n\n<li>mantenimento delle propriet\u00e0 elettriche o meccaniche dopo il condizionamento.<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">Un basso assorbimento d&#039;acqua non significa nemmeno una trasmissione di vapore acqueo pari a zero. Il silicone ha una trasmissione relativamente elevata. <a href=\"https:\/\/rysilicone.com\/it\/silicones-gas-permeability\/\">permeabilit\u00e0 ai gas e ai vapori<\/a> Rispetto a molti elastomeri organici densi, questa caratteristica \u00e8 utile per le membrane traspiranti, ma pu\u00f2 rappresentare un limite negli imballaggi con barriera all&#039;umidit\u00e0 o negli involucri dei sensori.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Come dovrebbero specificare gli acquirenti la densit\u00e0 del silicone?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Utilizzare la densit\u00e0 come una propriet\u00e0 controllata all&#039;interno di una specifica completa del materiale.<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Elemento di specifica<\/th><th>Requisito pratico<\/th><\/tr><\/thead><tbody><tr><td>Grado del materiale<\/td><td>Fornitore e codice esatto del composto<\/td><\/tr><tr><td>Sistema di cura<\/td><td>Sistema a platino, perossido o specifico per grado<\/td><\/tr><tr><td>Densit\u00e0 o peso specifico<\/td><td>Valore nominale e tolleranza secondo le specifiche tecniche approvate<\/td><\/tr><tr><td>Metodo di prova<\/td><td>ASTM D792, ASTM D297 o ISO 1183-1<\/td><\/tr><tr><td>Condizioni di prova<\/td><td>Temperatura, condizioni del campione e stato di polimerizzazione<\/td><\/tr><tr><td>Tolleranza di peso parziale<\/td><td>Definita separatamente dalla densit\u00e0 del materiale<\/td><\/tr><tr><td>Fabbisogno idrico<\/td><td>Test di assorbimento, immersione, pressione, trasmissione del vapore o IP<\/td><\/tr><tr><td>Cambiare controllo<\/td><td>Nessuna modifica alla formulazione o sostituzione degli eccipienti senza autorizzazione.<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Non utilizzare la sola densit\u00e0 per scegliere un composto siliconico. Due materiali possono avere la stessa densit\u00e0 pur differendo per resistenza alla trazione, resistenza allo strappo, deformazione permanente da compressione, requisiti di post-polimerizzazione, sostanze estraibili e conformit\u00e0 normativa.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Domande frequenti<\/h2>\n\n\n<div id=\"rank-math-faq\" class=\"rank-math-block\">\n<div class=\"rank-math-list\">\n<div id=\"faq-question-1785808566965\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\">Il silicone alimentare galleggia?<\/h3>\n<div class=\"rank-math-answer\">\n\n<p>Il contatto con gli alimenti non determina la galleggiabilit\u00e0. La maggior parte dei componenti in silicone solido destinati al contatto con gli alimenti affondano perch\u00e9 la loro densit\u00e0 \u00e8 superiore a 1,00 g\/cm\u00b3. Un componente cavo o espanso pu\u00f2 galleggiare.<\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1785808576522\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\">Il silicone \u00e8 pi\u00f9 pesante dell&#039;acqua?<\/h3>\n<div class=\"rank-math-answer\">\n\n<p>La maggior parte della gomma siliconica solida \u00e8 pi\u00f9 pesante dell&#039;acqua dolce per unit\u00e0 di volume. La densit\u00e0 tipica di un composto \u00e8 di circa 1,05\u20131,60 g\/cm\u00b3, mentre quella dell&#039;acqua dolce \u00e8 vicina a 1,00 g\/cm\u00b3.<\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1785808583630\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\">Una maggiore durezza Shore implica una maggiore densit\u00e0?<\/h3>\n<div class=\"rank-math-answer\">\n\n<p>Non necessariamente. Sia la durezza che la densit\u00e0 dipendono dalla formulazione, ma non esiste una conversione universale tra di esse. Utilizzare la TDS (solidi totali disciolti) del composto per ciascun valore.<\/p>\n\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n\n\n<h2 class=\"wp-block-heading\">Il confine del design<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Per i calcoli del peso, fornire il volume CAD finale, il peso dell&#039;inserto, la densit\u00e0 del composto approvata e la tolleranza di peso del pezzo. Per la flottazione, fornire la massa completa dell&#039;assemblaggio, il volume esterno spostato, il metodo di sigillatura della cavit\u00e0 e il liquido di servizio. Per la resistenza all&#039;acqua, definire pressione, tempo, temperatura, geometria del giunto e la prova applicabile.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Senza tali informazioni, affermazioni come &quot;il silicone galleggia&quot; e &quot;il silicone \u00e8 impermeabile&quot; sono generalizzazioni sui materiali, non specifiche di produzione.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Riferimenti tecnici<\/h2>\n\n\n\n<ul class=\"wp-block-list\">\n<li><a href=\"https:\/\/www.wacker.com\/h\/en-bg\/medias\/6709-EN.pdf\" target=\"_blank\" rel=\"noopener\">WACKER: Gomma siliconica solida e liquida \u2014 Linee guida per materiali e processi<\/a><\/li>\n\n\n\n<li><a href=\"https:\/\/www.simtec-silicone.com\/blogs\/why-only-hollow-lsr-parts-float-on-water\/\" target=\"_blank\" rel=\"noopener\">SIMTEC: Perch\u00e9 solo i componenti LSR cavi galleggiano sull&#039;acqua<\/a><\/li>\n\n\n\n<li><a href=\"https:\/\/www.intertek.com\/polymers-plastics\/testlopedia\/density-and-specific-gravity-astm-d792\/\" target=\"_blank\" rel=\"noopener\">Intertek: Densit\u00e0 e peso specifico \u2014 ASTM D792 e ISO 1183<\/a><\/li>\n\n\n\n<li><a href=\"https:\/\/www.intertek.com\/polymers-plastics\/testlopedia\/water-absorption-astm-d570\/\" target=\"_blank\" rel=\"noopener\">Intertek: Assorbimento d&#039;acqua \u2014 ASTM D570<\/a><\/li>\n\n\n\n<li><a href=\"https:\/\/pubs.acs.org\/doi\/10.1021\/acs.langmuir.0c00538\" target=\"_blank\" rel=\"noopener\">Bagnabilit\u00e0 adattiva del polidimetilsilossano, Langmuir<\/a><\/li>\n<\/ul>","protected":false},"excerpt":{"rendered":"<p>Silicone is often described as lightweight, waterproof, and hydrophobic. Those terms are easy to mix up. Typical solid silicone density is about 1.05\u20131.60 g\/cm\u00b3, so most unfoamed silicone parts sink in water. Hydrophobicity helps water bead on the surface, but it does not make every silicone design leakproof or impermeable. For product design, three separate [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":18815,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[],"class_list":["post-18813","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-uncategorized"],"_links":{"self":[{"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/posts\/18813","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/comments?post=18813"}],"version-history":[{"count":2,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/posts\/18813\/revisions"}],"predecessor-version":[{"id":18933,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/posts\/18813\/revisions\/18933"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/media\/18815"}],"wp:attachment":[{"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/media?parent=18813"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/categories?post=18813"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/rysilicone.com\/it\/wp-json\/wp\/v2\/tags?post=18813"}],"curies":[{"name":"parola chiave","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}